For most commercial applications the 15 mil thick concrete vapor barrier will be a better choice.
Concrete slab vapor barrier repair.
All vapor barriers should conform to astm e 1745.
Cure with waterproof sheets rather than with water or curing compounds.
But they have also proven to be beneficial in reducing failures of moisture sensitive flooring materials adhesives and coatings caused by excessive emission of moisture vapor from concrete slabs.
To minimize cracking on top of vapor barriers use a 100 mm thick 4 in layer of slightly damp compactible drainable fill choked off with fine grade material.
Studies have shown that vapor barriers can affect the behavior of the concrete slab and significantly influence finishing time cracking and strength.
Another solution is the new vaporstake that seals to the vapor barrier and is then cut off and left in the slab.
If you want to make sure your slab on ground gets dry and stays dry use a vapor barrier.
Architects engineers and contractors therefore often disagree on whether concrete should be placed directly on the vapor barrier or on a granular base placed over the vapor barrier.
However the current practice recommended by the american concrete institute is to apply a heavy grade non penetrable vapor barrier or retarder with the lowest possible permeance for the application over a layer of granular fill crushed rock gravel etc.
Some supports come with wide bearing pads.
For most residential applications the 10 mil under slab vapor barrier will offer enough protection against moisture vapor transmission coming up through the concrete floor allowing for flooring materials to be successfully installed on top of the concrete.
It successfully alleviates the problems associated with moisture accumulation in a concrete slab keeping moisture from reaching the epoxy flooring system.
Choosing a vapor barrier.
The concrete slab is then poured on top of it.
If concrete must be placed directly on polyethylene sheet or other vapor barriers placed directly on polyethylene sheet or other vapor barriers use a mix with a low water content.
Vapor barriers have been associated with certain concrete slab on grade problems including curling and cracking.
Seams should overlap 6 inches.
Water vapor diffusing through the concrete slab can also lead to deformation and discoloration of the floor covering material leading to costly repairs or even replacement.
The number of primer barrier layers is based on the amount of moisture present in concrete.
The moisture vapor barrier helps reduce the passage of fluids through concrete.
Water below the concrete slab can diffuse through the slab as vapor then condense under the flooring which can emulsify some adhesive and destroy the floor covering.